Denizli Light Travertine
Petrographical Properties:

The sample consists of calcite crystals with grain sizes between 30-100 microns and a micritic mud of 1-4 grain sizes.


Turkish

American
Physical, Mechanical and Technological Specifications
Hardness (mohs) 4
Unit Volume by weight (gr/cm3) 2,50
Density (gr/cm3) 2,72
Water Absortion at Atmospheric Pressure (by weight %) 1,0
(by volume %) 2,3
Water Absorption at Boiling Water (by weight %) 1,2
(by volume %) 3,0
Prosity (%) 2,3
Compressive Strenght (Kgf/cm2) 570
Compresssive Strenght After Freezing (Kgf/cm2) 582
Strenght to Blow (Kgf/cm/cm3) 11
Strenght to bending (Kgf/cm2) 108
Modules of Elasticity (Kgf/cm2) 5,38x104
Ratio of Fullness (%) 91,9
Degree of Pores (%) 8,1
Average Abrasion Strenght (cm3/50 cm2) 28,7
Average Tensile Strenght (Kgf/cm2) 41
     
Chemical Analysis %
SiO2 0,26
Fe2O3 0,32
CaO 54,55
MgO 0,31
 